羅萍 戴小紅 賀軍軍 李剛 張華林
摘 要 對(duì)天然橡膠品系紅星1開(kāi)展了氣刺微割試驗(yàn)。結(jié)果表明:采用氣刺微割后,紅星1的產(chǎn)量較穩(wěn)定,5 a平均凈增產(chǎn)率達(dá)7.00%,對(duì)干含影響不明顯;氣刺割膠采膠時(shí)間比傳統(tǒng)割膠少用0.6 h,節(jié)省勞動(dòng)時(shí)間13.9%,微割的耗皮僅為常規(guī)割膠的35%~40%。但長(zhǎng)流膠和死皮現(xiàn)象較為明顯,需引起重視。
關(guān)鍵詞 橡膠樹(shù) ;紅星1 ;氣刺微割 ;適應(yīng)性
中圖分類號(hào) S794.1 文獻(xiàn)標(biāo)識(shí)碼 A Doi:10.12008/j.issn.1009-2196.2017.08.001
Abstract A gas-stimulated micro-tapping system trial was conducted for rubber plantations of rubber clone Hongxing1. The results showed that the rubber plantations of the clone Hongxing1 tapped under gas-stimulated micro-tapping system yielded stable with an annual yield rate of 7.00% over 5 years of tapping. And there was no significant effect on dry rubber content. The gas-stimulated micro-tapping system had no significant impact on dry rubber content, and saved tapping time by 0.6 hour per tree, labor by 13.9% and bark by 35~40% as compared to the conventional tapping system. But late dripping and tapping panel dryness incidence were obviously observed in the trial, which should be taken into account.
Keywords rubber tree ; clone Hongxing1 ; gas-stimulated micro-tapping system ; adaptability
氣刺微割技術(shù)是20世紀(jì)90年代初馬來(lái)西亞橡膠研究院研發(fā)的[1]。此項(xiàng)技術(shù)可大幅度提高勞動(dòng)生產(chǎn)率并減少膠樹(shù)耗皮,延遲橡膠樹(shù)采膠年限,對(duì)割膠生產(chǎn)具有重要意義[1]。中國(guó)從1995年開(kāi)始進(jìn)行氣刺微割技術(shù)試驗(yàn),經(jīng)過(guò)10多年的研究,現(xiàn)已基本掌握了氣刺割膠的技術(shù)特點(diǎn)和操作要領(lǐng)[1]。氣刺微割是一種安全、高效和可持續(xù)的采膠技術(shù)[2],具有割線短、省樹(shù)皮、延割齡、提工效、降成本的特點(diǎn),目前已在中國(guó)幾個(gè)主產(chǎn)膠區(qū)逐步推廣。廣東植膠區(qū)開(kāi)始?xì)獯淘囼?yàn)較晚,從2006年以來(lái),廣東墾區(qū)圍繞提高割膠勞動(dòng)生產(chǎn)率和單位面積產(chǎn)量,促進(jìn)企業(yè)增效和職工增收,積極探索氣刺微割技術(shù)在廣東植膠區(qū)的應(yīng)用和推廣,在下屬的湛江、茂名部分農(nóng)場(chǎng)陸續(xù)開(kāi)展氣刺微割田間試驗(yàn),試驗(yàn)總規(guī)模達(dá)16 000多株[3]。為了該技術(shù)在廣東墾區(qū)更好地推廣應(yīng)用,從2008年開(kāi)始,國(guó)家天然橡膠產(chǎn)業(yè)技術(shù)體系湛江綜合試驗(yàn)站在徐聞縣五一農(nóng)場(chǎng)開(kāi)展氣刺短線割膠技術(shù)試驗(yàn),著重考察了氣刺微割技術(shù)對(duì)天然橡膠品系紅星1的產(chǎn)膠情況及膠樹(shù)生理性狀等方面的影響,以期為該技術(shù)在生產(chǎn)上的推廣應(yīng)用提供依據(jù)。
1 材料與方法
1.1 材料
采用30割齡的紅星1品系,包括6個(gè)樹(shù)位,試驗(yàn)面積4.8 hm2,株數(shù)1 500株。
1.2 方法
1.2.1 試驗(yàn)設(shè)計(jì)
試驗(yàn)地點(diǎn)位于廣東省徐聞縣國(guó)營(yíng)五一農(nóng)場(chǎng)9隊(duì)的國(guó)家天然橡膠產(chǎn)業(yè)技術(shù)體系湛江綜合試驗(yàn)站氣刺短線割膠技術(shù)試驗(yàn)示范基地。試驗(yàn)時(shí)間為2009~2013年。試驗(yàn)設(shè)3次重復(fù),選擇3個(gè)割膠技術(shù)相近的膠工,每個(gè)膠工負(fù)責(zé)1個(gè)重復(fù),包括1個(gè)處理樹(shù)位和1個(gè)對(duì)照樹(shù)位。對(duì)照與處理選擇割齡相當(dāng)、土壤地力水平相似、品系、割頻均相同的相鄰樹(shù)位。處理采用S/8d/4+ET(氣體)割制,每3刀換1次氣。對(duì)照采用(S/4+S/4↑)d/4+ET3.5%割制,試驗(yàn)期間每年安排割48刀,4刀為1個(gè)周期,共12周期。2009~2010年采用軟質(zhì)氣室,2011~2013年采用硬質(zhì)氣室,2012~2013年配套防雨帽割膠。
1.2.2 調(diào)查內(nèi)容
每次割膠收膠結(jié)束后,測(cè)量每個(gè)樹(shù)位的流膠量、長(zhǎng)流膠量及干含,每隔1個(gè)月對(duì)病蟲(chóng)害進(jìn)行觀察統(tǒng)計(jì)1次,停割后對(duì)死皮情況進(jìn)行觀察和記錄。于2013年開(kāi)割以后,對(duì)2種割制的樹(shù)皮進(jìn)行觀察,每個(gè)周期定期對(duì)樹(shù)皮厚度、樹(shù)皮顏色、木柵化程度、死皮情況、樹(shù)皮開(kāi)裂、流膠時(shí)間等情況進(jìn)行觀察記錄,調(diào)查株數(shù)為30株。2013年開(kāi)割后第4個(gè)周期,于每次割膠后每小時(shí)對(duì)膠乳濃度進(jìn)行測(cè)定,調(diào)查株數(shù)為9株。
2 結(jié)果與分析
2.1 產(chǎn)量情況
紅星1產(chǎn)量比較穩(wěn)定,有一定的增產(chǎn)效果,單株平均產(chǎn)膠為0.98 kg,增產(chǎn)率為7.00%,增產(chǎn)干膠0.08 kg,近5 a的產(chǎn)量情況見(jiàn)表1。
2013年紅星1各周期產(chǎn)量曲線圖見(jiàn)圖1。由圖1可知,紅星1品系采用氣割制的樹(shù)位產(chǎn)量比較穩(wěn)定,割膠第1個(gè)周期產(chǎn)量為0.09 kg/株,隨后產(chǎn)量逐漸提高,到第8周期的時(shí)候產(chǎn)量達(dá)到峰值,平均產(chǎn)量為0.22 kg/株,與第1周期相差0.13 kg,到8月份受到臺(tái)風(fēng)的影響,產(chǎn)量下降到0.17 kg;采用傳統(tǒng)割制的產(chǎn)量波動(dòng)比較大,第1周期平均產(chǎn)量為0.15 kg/株,第7周期平均產(chǎn)量為0.43 kg/株,前期和中期相差0.28 kg。endprint
2.2 勞動(dòng)效率
2013年對(duì)紅星1品系進(jìn)行田間調(diào)查,每個(gè)樹(shù)位約250株膠樹(shù),結(jié)果見(jiàn)表2。采用傳統(tǒng)割制的樹(shù)位平均采膠時(shí)間為4.3 h,采用氣刺割制的樹(shù)位平均采膠時(shí)間為3.7 h。在割膠時(shí)間方面,采用氣割的樹(shù)位比傳統(tǒng)割制少用1.1 h,節(jié)省勞動(dòng)時(shí)間34.4%。因此,采用氣刺割制在割膠方面能有效提高勞動(dòng)效率,節(jié)省割膠成本。2種割制在第1次收膠和采集膠絲時(shí)間方面沒(méi)有明顯區(qū)別,但在采收長(zhǎng)流膠方面,采用傳統(tǒng)割制的樹(shù)位用時(shí)為0.3 h,而采用氣刺割制的樹(shù)位用時(shí)為0.8 h,比前者多用0.5 h。因此,氣刺割制在長(zhǎng)流膠回收方面會(huì)用較多勞動(dòng)力??傮w來(lái)說(shuō),氣刺割制采膠時(shí)間比傳統(tǒng)割制少用0.6 h,節(jié)省勞動(dòng)時(shí)間13.9%。因此,氣刺割制能有效提高割膠勞動(dòng)效率,降低割膠成本。
2.3 干膠含量
常年采用氣刺割制對(duì)干膠含量也會(huì)造成一定的影響。不同品系采用氣刺割制以后干膠含量變化也不同。一般來(lái)說(shuō),耐刺激的品系經(jīng)過(guò)氣體刺激以后,在產(chǎn)量穩(wěn)定的情況下干含也比較穩(wěn)定,而且樹(shù)皮死皮及病變情況較少;不耐刺激的品系在經(jīng)過(guò)氣體刺激以后,干含會(huì)逐漸下降。
從試驗(yàn)結(jié)果來(lái)看(表3),氣刺微割對(duì)膠水干含的影響不是很大,紅星1試前S/8d/4+EG(氣體)割制下的平均干膠含量為25.1%,試后2013年為26.3%,相對(duì)于對(duì)照組,差異不明顯。膠乳的干膠含量通常為28%以上,但參試膠林的干膠含量低于這個(gè)水平,影響橡膠干含的因素很多,如氣溫變化、割膠制度、刺激和環(huán)境因素等,這些對(duì)試驗(yàn)的準(zhǔn)確性都會(huì)造成一定影響。
2.4 耗皮量
氣刺微割割線長(zhǎng)度為8~12 cm,年耗皮量?jī)H為120~144 cm2,而對(duì)照則達(dá)到350~450 cm2,微割的耗皮僅為常規(guī)割膠的35%~40%,可大大節(jié)省樹(shù)皮。
2.5 長(zhǎng)流膠情況
紅星1長(zhǎng)流膠產(chǎn)量情況見(jiàn)表4。由表4可知,傳統(tǒng)割制的長(zhǎng)流膠產(chǎn)量占干膠總產(chǎn)的1.42%;氣刺割制長(zhǎng)流膠產(chǎn)量占干膠總產(chǎn)的46.98%。以上數(shù)據(jù)說(shuō)明,傳統(tǒng)割制產(chǎn)生的長(zhǎng)流膠較少,一般不需要重復(fù)收膠,在收膠方面可以節(jié)省一定的勞動(dòng)力;氣刺割膠產(chǎn)生的長(zhǎng)流膠較多,需要重復(fù)收膠,在收膠方面需要投入更多的勞動(dòng)力。
氣刺微割后流膠時(shí)間見(jiàn)表5。由表5可知,氣刺割膠的平均流膠時(shí)間為23.2 h;傳統(tǒng)割制的平均流膠時(shí)間為7.6 h,與氣刺割制相差15.6 h。氣刺割制個(gè)別膠樹(shù)流膠時(shí)間最長(zhǎng)可達(dá)到74 h,傳統(tǒng)割制最長(zhǎng)流膠時(shí)間只有13.5 h;氣刺割制最短流膠時(shí)間為16.5 h,傳統(tǒng)割制最短流膠時(shí)間為4.5 h??梢?jiàn)氣刺割膠延長(zhǎng)了流膠時(shí)間。
2.6 膠乳干含變化情況
在流膠過(guò)程中,通常前期流膠速度較快,膠乳干含也較高,隨著流膠時(shí)間的增加,流膠速度會(huì)逐漸變慢,膠乳干含也會(huì)逐漸降低,最終流膠停止。
圖2是不同割制膠乳干含隨時(shí)間的變化情況。由圖2可知,傳統(tǒng)割制開(kāi)割時(shí)干含為25.8%,隨著時(shí)間的增加,干含逐漸降低,9 h時(shí),干含降到24.4%,最后流膠停止;氣刺割制流膠時(shí)間較長(zhǎng),在11 h時(shí),膠乳下降速度較快,到18 h時(shí)停止流膠,干含為23.3%。
2.7 死皮情況
橡膠樹(shù)死皮是指割線排膠影響面范圍內(nèi)的乳管系,由于生理或病理的原因,局部或全部喪失產(chǎn)膠機(jī)能的病變。死皮現(xiàn)象是橡膠樹(shù)割膠過(guò)程中常出現(xiàn)的一種情況,死皮原因有很多種,分為生理死皮和病理死皮,使用氣刺割膠以后也會(huì)對(duì)橡膠樹(shù)死皮情況產(chǎn)生一定影響,紅星1在使用氣刺割膠以后,新增死皮率有提高的現(xiàn)象。如表6所示,紅星1在2009年未出現(xiàn)4級(jí)死皮現(xiàn)象,2010年新增4級(jí)死皮率為0.25%,2011和2012年新增均為0.26%,使用傳統(tǒng)割制的2009~2012年未出現(xiàn)4級(jí)死皮現(xiàn)象。
由于采用氣刺割膠,使排膠時(shí)間延長(zhǎng),可能會(huì)導(dǎo)致樹(shù)皮過(guò)度疲勞,膠乳濃度變低,對(duì)樹(shù)皮產(chǎn)生傷害,從而加重死皮的發(fā)生。橡膠樹(shù)死皮病是干膠生產(chǎn)的嚴(yán)重障礙,它所造成的損失和臺(tái)風(fēng)對(duì)橡膠樹(shù)為害造成的損失相近。患死皮橡膠樹(shù)的割線,初期呈灰暗色水漬狀,嚴(yán)重時(shí)出現(xiàn)褐色斑點(diǎn),最后引起樹(shù)皮組織壞死,割面變形,樹(shù)皮干枯,爆裂脫落。據(jù)觀察,相當(dāng)部分的干涸病會(huì)發(fā)展為褐皮病。褐皮病發(fā)病初期出現(xiàn)的褐斑,以后會(huì)形成褐線,向割線兩側(cè)和排膠面方向擴(kuò)展,使成片的韌皮組織壞死。據(jù)觀察,死皮前也有相應(yīng)的癥狀,通常干膠含量持續(xù)下降,在臨界指標(biāo)24%~25%徘徊;排膠量驟增或長(zhǎng)流嚴(yán)重;割線局部早凝,膠乳外流;割線變色,如“熟番薯”狀,切割時(shí)有脆爽之感。
2.8 樹(shù)皮其他癥狀
2.8.1 樹(shù)皮變厚
采用氣刺割制以后,橡膠樹(shù)在刺激部位周圍出現(xiàn)樹(shù)皮均變厚的情況,紅星1在試驗(yàn)前的樹(shù)皮厚度為1.23 cm,試后樹(shù)皮的厚度增加到1.35 cm,厚度增加0.12 cm。
2.8.2 木柵化
調(diào)查的100株橡膠樹(shù)中,有98株出現(xiàn)木柵化現(xiàn)象,但割開(kāi)仍有膠水流出,可以繼續(xù)割膠。
2.8.3 樹(shù)皮開(kāi)裂
使用氣刺割膠以后,氣室周圍的樹(shù)皮出現(xiàn)樹(shù)皮開(kāi)裂的現(xiàn)象,表皮木柵化并死亡,從內(nèi)部長(zhǎng)出新的再生皮,一般不會(huì)出現(xiàn)死皮現(xiàn)象,再生皮可以繼續(xù)割膠。
2.9 防雨帽技術(shù)的應(yīng)用
采用氣刺微割以后,長(zhǎng)流膠的比例會(huì)增加,流膠時(shí)間也增加,在此情況下,很容易受到雨水的沖刷,使膠水造成更大的損失。而在安裝了防雨帽的樹(shù)位,2013年共被雨水淋了3次,挽回膠水267 kg。因此安裝防雨帽有助于解決被雨水沖膠水的問(wèn)題。
3 結(jié)論與討論
氣刺割膠主要是通過(guò)延長(zhǎng)橡膠樹(shù)的排膠時(shí)間而獲得產(chǎn)量[4]。采用氣刺微割可以減少膠樹(shù)的耗皮量、降低傷樹(shù)率、節(jié)省勞動(dòng)力、提高勞動(dòng)效率、降低割膠成本。S/8d/4+EG(氣體)割制的特點(diǎn)就是割線短,割線長(zhǎng)度為8~12 cm,耗皮僅為常規(guī)割膠的35%~40%,可大大節(jié)省樹(shù)皮,延長(zhǎng)膠樹(shù)的經(jīng)濟(jì)壽命。因在割膠時(shí)候比對(duì)照少割一段樹(shù)皮,膠工操作方便,割膠速度明顯提高,膠工的人均管理株數(shù)增加,勞動(dòng)收入也隨之增加。膠工月均收入由原來(lái)的1 000~1 300元提高到1 500~1 600元。采用氣刺割制,可使割膠勞動(dòng)力節(jié)省13.9%,每個(gè)樹(shù)位可以節(jié)省0.6 h的勞動(dòng)時(shí)間,按當(dāng)?shù)?元/h的工價(jià)來(lái)計(jì)算,每個(gè)樹(shù)位每次割膠可節(jié)省4.8元,一年60刀可以節(jié)省288元。endprint
采用氣刺微割的紅星1產(chǎn)量較穩(wěn)定,有一定的增產(chǎn)效果,對(duì)干含的影響也不大,但長(zhǎng)流膠現(xiàn)象明顯,應(yīng)引起重視。因產(chǎn)生的長(zhǎng)流膠較多,流膠時(shí)間較長(zhǎng),需要重復(fù)收膠,在收膠方面需要投入更多的勞動(dòng)力,同時(shí)應(yīng)做好防雨措施,如采用防雨帽技術(shù)等,以減少膠水損失。
由于氣刺微割的刺激強(qiáng)度比傳統(tǒng)割制的大,過(guò)度刺激容易導(dǎo)致死皮現(xiàn)象的發(fā)生,所以死皮的防治也是推廣該技術(shù)的重點(diǎn)和難點(diǎn)。死皮的防治要注意以下幾點(diǎn):一是通過(guò)調(diào)控刺激強(qiáng)度和采膠強(qiáng)度,使產(chǎn)膠與排膠保持動(dòng)態(tài)平衡。具體做法包括降低割膠頻率、縮短割線、施用低濃度低劑量乙烯利、輪換割面和增施肥料等;二是隔離病灶,使死皮停割樹(shù)復(fù)割。不論哪個(gè)割面,出現(xiàn)死皮癥狀后及時(shí)隔離病灶,合理復(fù)割則80%以上不復(fù)發(fā);三是淺刨病灶,施復(fù)方微量元素治療。選擇4~9月的晴天對(duì)死皮樹(shù)進(jìn)行刨皮處理,然后取鉬酸鍍10 g,硼砂10 g,硫酸鋅10 g,淀粉60~70 g,溶于少量溫水中,邊攪拌邊沖入100 mL沸水,即成糊狀藥液。用毛刷蘸藥液涂在刨皮面上,當(dāng)天刨皮當(dāng)天涂藥,一株病樹(shù)用藥量約100~150 mL;四是注意天氣變化,要看天割膠,防止雨沖膠,貫徹樹(shù)身、割面不干不割,危險(xiǎn)天氣不割或高、中產(chǎn)樹(shù)不割的措施。發(fā)病后應(yīng)在割膠時(shí)使割皮厚些,盡快把病皮割完,以免擴(kuò)展。
從上述試驗(yàn)結(jié)果可以看出,采用氣刺割膠以后在前幾年會(huì)出現(xiàn)增產(chǎn)的現(xiàn)象,而在往后幾年出現(xiàn)減產(chǎn)的現(xiàn)象,說(shuō)明膠樹(shù)在增產(chǎn)的同時(shí)也耗費(fèi)了大量營(yíng)養(yǎng),死皮、樹(shù)皮病變、干含降低等現(xiàn)象也隨之而來(lái),所以要養(yǎng)樹(shù)割膠。中國(guó)割膠生產(chǎn)的經(jīng)驗(yàn)表明,要保持橡膠樹(shù)的高產(chǎn)穩(wěn)產(chǎn),必須將挖掘產(chǎn)膠潛力和保護(hù)橡膠樹(shù)的產(chǎn)膠潛力有機(jī)地結(jié)合起來(lái),就是說(shuō)既要割膠又要養(yǎng)樹(shù)。割膠的目的是獲取產(chǎn)量,養(yǎng)樹(shù)是獲得持久高產(chǎn)的保證,這樣才能既高產(chǎn)又減少死皮的發(fā)生。
參考文獻(xiàn)
[1] ?,F(xiàn)周,魏小弟,羅世巧,等. 論橡膠樹(shù)氣刺微割技術(shù)發(fā)展戰(zhàn)略[J]. 熱帶農(nóng)業(yè)科學(xué),2007,27(2):52-53.
[2] 劉實(shí)忠,?,F(xiàn)周,魏小弟,等. 中國(guó)氣刺微割研究現(xiàn)狀[J]. 熱帶農(nóng)業(yè)科學(xué),2010,30(8):42-45.
[3] 李小園,陳葉海. 橡膠樹(shù)氣刺微割采膠技術(shù)應(yīng)用推廣初報(bào)[J]. 熱帶農(nóng)業(yè)科學(xué),2010,30(8):55-58.
[4] 校現(xiàn)周,羅世巧,魏小弟. 橡膠樹(shù)氣刺割膠新進(jìn)展[J]. 熱帶農(nóng)業(yè)科學(xué),2010,30(8):68-70.endprint